SR EN 10213-4:1996
Technical delivery conditions for steel casting for pressure purposes. Part 4: Austenitic and austenitic-ferritic steel grades
According to the general delivery conditions of EN 10213-1 this standard specifies the chemical and mechanical requirements to be met under specific inspection of austenic and austenitic-ferritic grades.
You must log in to add this product to favorites.
Status :
Withdrawn
Approval date : 8/9/1996
Publish date : 8/10/1996
Withdrawal date : 5/31/2008
Number of pages : 10
ICS : 77.140.10 Heat-treatable steels,77.140.30 Steels for pressure purposes
Technical Committee : 47 - Foundry technology
- Normative reference SR EN 10213-1:1996
- Replaced by SR EN 10213:2008